Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Polimeri Europa Clearflex® MQ F0 Very Low Density Polyethylene Clearflex MQ F0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | At 100% elongation, across flow; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-75 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D412 |
Polymax® Maxelast® P1870 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 4.00 - 369 MPa | 580 - 53500 psi | Average value: 32.1 MPa Grade Count:775 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 85U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Support Rubber |
Fujipoly Industries Zebra® Silver Connector Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 50 mm/min; ISO 527-1/-2 |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-55-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B500 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B700 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg R608 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Z800 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Z900 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 5143S Homopolymer Polypropylene Homopolymer for Extrusion Sheet and Thermoforming Applications Formolene® 5143S is a higher melt flow homopolymer designed for light weighting of components. Its very high stiffness enables reducti.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg B600 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 4.00 MPa @Strain 50.0 % |
580 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Nakan® FMM 611 N PVC, Soft Injection Molding Grade NAKAN FMM 611 N is a soft polyvinyl chloride compound developed for injection molding of breathing masks and general purpose.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Film Property, 50 µm thickness; ASTM D882 |
Arkema Group OREVAC® 9304 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
ACC MM230 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: ceramic/polyester/PU/epoxy a.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
ACC MM239 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: ceramic/polyester/PU/epoxy a.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | 50 mm/min |
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy .. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
BASF Lucalen® A 2710 H Ethylene/Acrylate Copolymer Product with properties which are typical of flexible PVC and of low density polyethylene. Suitable for flexible pipes, profiles and seals.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | |
Trelleborg Z600 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 4.00 MPa @Strain 300 % |
580 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 37-023 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation .. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ASTM D638 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Breplast Bretene SP Polypropylene / Polyethylene Composite Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | ISO 527 |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |
|||
Tensile Strength, Yield | 4.00 MPa | 580 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |