Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 383 MPa @Strain 0.200 % |
55500 psi @Strain 0.200 % |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 383 MPa @Strain 0.200 % |
55500 psi @Strain 0.200 % |
|
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, Solution Treated Tensile strength (ultimate and yield), and elongation values reported here are typical for Cold Rolled Sheet, Solution Treated samples. Density and magnetic permeability are typical of annealed INCO.. |