Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 34.5 MPa | 5000 psi | 2 in per min, tangent; ASTM D638 |
Network Polymers NPP 30-3500 NA Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 8910 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 15 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D1457 |
Greene Tweed Avalon® 1 PTFE Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D882-83, Method A |
Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. T.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Techmer ES HiFill FR® ABS GB10 FR 10% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Techmer ES HiFill® ABS GB15 15% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | |
Saint-Gobain Rulon® 954 Bearing/Seal PTFE A conductive PTFE material that is available in tape, sheet (extruded) and rod (extruded).Information provided by distributor TriStar Plastics Corp. |
|||
Tensile Strength, Yield | 34.5 - 49.6 MPa | 5000 - 7200 psi | ASTM D-882 |
Saint-Gobain Norton® PVDF Fluoropolymer Film Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | 50 mm/min; ASTM D638 |
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 829-01 is a homopolymer polypropylene approved to Ford specification ESB-M4D63A. Primarily used for interior automotive components, this material is also well suited for.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | 50mm/min; ISO 527-2 |
Borealis HE125MO Polypropylene HE125MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by good flow properties and high stiffness in and is specially suitable for high-speed injection mo.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 3489-01 Polypropylene Homopolymer DescriptionPolypropylene PP 3489-01 is a specially designed homopolymer with excellent stiffness properties. ApplicationTypical applications include high speed extrusion, high speed thin wall injec.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Washington Penn Homopolymer Polypropylene 40% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Washington Penn Homopolymer Polypropylene 50% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Westlake Plastics Kynar® 2850 PVDF Copolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, r.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 5100H Extrusion processing Polypropylene HomopolymerApplications: Various extrusion profile, sheet and film applications.Formolene 5100H DEVELOPMENTAL is a high molecular weight, highly isotactic polypropylene homopolymer designed for vari.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, r.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 15 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Asahi Kasei Thermofil P-20TC-5100R 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | |
Asahi Kasei Thermylene® P-9900-0712 Chemically Coupled Polypropylene Compound Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 34.5 MPa @Temperature 23.0 °C |
5000 psi @Temperature 73.4 °F |
2 in/min; ASTM D638 |
Ineos H20E-00 Polypropylene Homopolymer This is a homopolymer containing antistatic designed for injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Application.. |