Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.5 MPa @Temperature 23.0 °C |
4860 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H03G-04 Polypropylene Homopolymer This is a polypropylene homopolymer for biaxially oriented polypropylene (BOPP) film and blow molding applications. This material meets the requirements of the U.S. Food and Drug Administration as .. |
|||
Tensile Strength, Yield | 33.5 MPa | 4860 psi | ISO 527-2 |
Borealis HB600TF Polypropylene HB600TF is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master batch without .. |
|||
Tensile Strength, Yield | 33.5 MPa | 4860 psi | 50mm/min; ISO 527-2 |
Borealis HD120MO Polypropylene HD120MO is a polypropylene homopolymer with a good combination of mechanical properties intended for injection molding. Applications: sanitary equipment, caps and closures, and general packagingInf.. |
|||
Tensile Strength, Yield | 33.5 MPa | 4860 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 33.5 MPa | 4860 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |