Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 324 MPa | 47000 psi | |
Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Yield | 324 MPa | 47000 psi | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-200-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Tensile Strength, Yield | 324 MPa @Temperature 93.3 °C |
47000 psi @Temperature 200 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 324 MPa | 47000 psi | |
Kinetics MIM 4605 Low Alloy Steel (As Sintered) Low alloy steel, carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness, and wear resistance properties depending if it is heat treated and the heat .. |
|||
Tensile Strength, Yield | 324 MPa @Strain 0.200 %, Temperature 538 °C |
47000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 324 - 469 MPa | 47000 - 68000 psi | 0.2% offset |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Yield | 324 MPa | 47000 psi | |
Chicago Extruded Metals BioBrass® UNS C27450 Copper-Zinc Alloy Finished product available as wire or tube.Chicago Extruded Metal temper code: H04Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 324 MPa @Temperature 482 °C |
47000 psi @Temperature 900 °F |
|
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536 Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu.. |
|||
Tensile Strength, Yield | 324 MPa | 47000 psi | |
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |
|||
Tensile Strength, Yield | 324 MPa | 47000 psi | |
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc.. |
|||
Tensile Strength, Yield | 324 MPa @Strain 0.200 %, Temperature 538 °C |
47000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Yield | 324 MPa @Strain 0.200 % |
47000 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Tensile Strength, Yield | 324 MPa @Strain 0.200 % |
47000 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |