Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 321 MPa @Strain 0.200 %, Temperature 816 °C |
46600 psi @Strain 0.200 %, Temperature 1500 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Tensile Strength, Yield | 321 MPa @Strain 0.200 % |
46600 psi @Strain 0.200 % |
|
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Yield | 321 MPa @Strain 0.200 % |
46600 psi @Strain 0.200 % |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Yield | 321 MPa @Temperature 70.0 °C |
46600 psi @Temperature 158 °F |
transverse |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-7 (UNS S20153) AL 201LN™ is a special composition of Type 201 specifically for sub-zero temperature service as welded tanks and vessels. This alloy has replaced the familiar 300 series stainless such as type 301.. |
|||
Tensile Strength, Yield | 321 MPa | 46600 psi | Typical |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |