Mechanical Properties Metric English Comments
Tensile Strength, Yield 313 MPa

@Strain 0.200 %,
Temperature 816 °C
45400 psi

@Strain 0.200 %,
Temperature 1500 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Tensile Strength, Yield 313 MPa

@Strain 0.200 %
45400 psi

@Strain 0.200 %
Typical Annealed
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed)
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci..
Tensile Strength, Yield 313 MPa

@Strain 0.200 %
45400 psi

@Strain 0.200 %
typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Annealed
Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles..