Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 311 MPa @Strain 0.200 %, Temperature 760 °C |
45100 psi @Strain 0.200 %, Temperature 1400 °F |
|
Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched Typical applications include, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc. |
|||
Tensile Strength, Yield | 311 MPa @Strain 0.200 % |
45100 psi @Strain 0.200 % |
|
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |