Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 31.5 MPa | 4570 psi | ASTM D638 |
NOVA Chemicals Sclair® 59E HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 31.5 MPa | 4570 psi | ASTM D638 |
NOVA Chemicals Sclair® 59F HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 31.5 MPa | 4570 psi | ASTM D638 |
IRPC Polimaxx Polene GM2860 High Density Polyethylene CHARACTERISTICS: HIGH IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH STIFFNESSAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES COSMETIC BOTTLES, ONE-WAY BOTT.. |
|||
Tensile Strength, Yield | 31.5 MPa | 4570 psi | ASTM D412 |
C.O.I.M. LARIPUR® LPR6518 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tensile Strength, Yield | 31.5 MPa | 4570 psi | ASTM D638 |
NOVA Chemicals Sclair® 59D HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |