Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Multibase Multi-Pro® 2010 M Polypropylene Mica Filled, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Multibase Multi-Pro® 4006 TH Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Multibase Multi-Pro® 4012 TH Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | ASTM D638 |
Flint Hills AP5206-HN Polypropylene Impact Copolymer Features: Nucleated for fast cycle and good mold release. Product does not contain animal derived components.Applications: Compression and injection molding: caps and closuresInformation Provided b.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Global CPP-110 10% CaC03 Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | 2 in/min (50 mm/min); ASTM D-638 |
Ineos H20A-00 Polypropylene Homopolymer A controlled rheology polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications requiring a moderate level of antistatic ag.. |
|||
Tensile Strength, Yield | 30.3 MPa @Temperature 23.0 °C |
4400 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos L06Z-00 Polypropylene Impact Copolymer This is a medium MFR impact copolymer polypropylene made for injection molded caps and closures applications. It offers a good balance of stiffness to impact resistance as compared to other impact .. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Kostat ICP-STAT ICD-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Techmer ES HiFill® HDPE TM30 30% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Spartech EP5220 Calcium Carbonate Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Calcium Carbonate filled grades offer an excellent balance of stiffness and impact resistance. Typical applications inc.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Spartech PE4312 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Spartech Royalstatâ„¢ R64 HDPE Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Techmer ES Plastiblend® ABS 8004 FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Techmer ES Luriblend® ABS TL2 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 3335N Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3335N is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for thin walled, injec.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Total HDPE B5845 High Density Polyethylene - Blow Molding Resin Bimodal HDPE Blow Molding ResinCharacteristics:Excellent stress cracking resistanceExcellent stiffnessApplications:Household chemicalsIndustrial chemicalsIndustrial partsFood packagingPersonal care .. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 572A1V95316 Cellulose Acetate Butyrate, Smoke, Trsp Applications:Molded partsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm fee.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | chs 2.0 in/min; tangent; ASTM D638 |
Diamond Polymers NPP25-1602 TF40 40% Talc Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Clariant ABSSP0004 ABS, Chemical Resistant Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Asahi Kasei Thermylene® P-20-0739 20% Talc Filled, High Impact, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4390 psi | ASTM Data |
Styron Magnum™ AG700 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |