Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 30.1 MPa | 4370 psi | ASTM D638 |
Petromont 1100 High Density Polyethylene Resin Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b.. |
|||
Tensile Strength, Yield | 30.1 MPa | 4360 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® M6028 High Density Polyethylene ApplicationsM 6028 is a homopolymer that is warp resistant, exhibits excellent toughness, stiffness and color as well as low odor and good processing stability. Typical applications include safety .. |
|||
Tensile Strength, Yield | 30.1 MPa | 4360 psi | ASTM D412 |
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU PEARLTHANE® CLEAR 15N70 is a polyether copolymer-based TPU with Shore 72 A hardness, free of plasticizer, supplied in form of translucent, colorless pellets with very low yellowness index. PEARLT.. |
|||
Tensile Strength, Yield | 30.1 MPa | 4360 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera.. |
|||
Tensile Strength, Yield | 30.1 MPa | 4370 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 30.1 MPa | 4370 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |