Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 30.05 MPa | 4359 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 18VT80 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and superior hydrolysis and microbe resistan.. |
|||
Tensile Strength, Yield | 30.05 MPa | 4359 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Tensile Strength, Yield | 30.05 MPa | 4359 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Tensile Strength, Yield | 30.05 MPa | 4359 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 165K Thermoplastic Polyurethane Elastomer PEARLCOAT® 165K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Tensile Strength, Yield | 30.05 MPa | 4359 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |