Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.52 MPa | 511 psi | at 200%, as molded |
Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.52 MPa | 510 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4565 VAROX Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.52 MPa | 510 psi | at 100%; ASTM D412 |
2074A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 3.52 MPa | 510 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.52 MPa | 511 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tensile Strength, Yield | 3.52 MPa | 511 psi | cured 7 mins @ 150°C |
ACC QSil 550 QSI Quantum Silicones Silicone Potting Material QSil 550 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab.. |
|||
Tensile Strength, Yield | 3.52 MPa | 510 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3630 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 3.52 MPa @Strain 100 % |
511 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ HTE 1106 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) |