Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.105 MPa | 450.3 psi | -25% change after 336 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S50E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci.. |
|||
Tensile Strength, Yield | 3.105 MPa | 450.3 psi | -25% change after 336 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S60E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 55-65 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci.. |