Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 283 MPa @Strain 0.200 % |
41000 psi @Strain 0.200 % |
|
FloMet 7% Ni/Fe Low Alloy Steel FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Yield | 283 MPa @Strain 0.200 %, Temperature 427 °C |
41000 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Ultimet® alloy, 1.6 mm sheet Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 283 MPa @Strain 0.200 %, Temperature 427 °C |
41000 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | >= 283 MPa | >= 41000 psi | |
Alcoa UltrAlloy® 6020-T8 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Tensile Strength, Yield | 283 - 345 MPa | 41000 - 50000 psi | 0.2% offset |
Eagle Brass 110 EPT COPPER, Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Yield | 283 - 345 MPa | 41000 - 50000 psi | 0.2% offset |
Eagle Brass 101 OFE COPPER (Certified), Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Yield | 283 - 345 MPa | 41000 - 50000 psi | 0.2% offset |
Eagle Brass 102 OF COPPER (Non-Certified), Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Yield | >= 283 MPa @Strain 0.200 % |
>= 41000 psi @Strain 0.200 % |
|
Carlson GOC 276 Nickel-Molybdenum-Chromium General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in .. |
|||
Tensile Strength, Yield | 283 MPa @Strain 0.200 % |
41000 psi @Strain 0.200 % |
|
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Yield | >= 283 MPa @Strain 0.200 % |
>= 41000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276 AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encount.. |
|||
Tensile Strength, Yield | 283 MPa @Strain 0.200 %, Temperature 760 °C |
41000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Yield | 283 MPa @Strain 0.200 %, Temperature 204 °C |
41000 psi @Strain 0.200 %, Temperature 399 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |