Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 280 MPa @Strain 0.200 %, Temperature 538 °C |
40600 psi @Strain 0.200 %, Temperature 1000 °F |
|
Kennametal Stellite Stellite® 31 PM cast Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we.. |
|||
Tensile Strength, Yield | 280 - 720 MPa @Strain 0.200 % |
40600 - 104000 psi @Strain 0.200 % |
|
Materion Brush 1915â„¢ Annealed Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Yield | 280 MPa @Strain 0.200 % |
40600 psi @Strain 0.200 % |
Annealed prior to test |
Special Metals INCOLOY® Alloy 330 A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher.. |
|||
Tensile Strength, Yield | 280 - 350 MPa @Strain 0.200 % |
40600 - 50800 psi @Strain 0.200 % |
|
SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Tensile Strength, Yield | 280 - 350 MPa @Strain 0.200 % |
40600 - 50800 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 280YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Tensile Strength, Yield | 280 - 450 MPa @Strain 0.200 % |
40600 - 65300 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 600DL High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Tensile Strength, Yield | >= 280 MPa @Strain 0.200 % |
>= 40600 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® DC01 (Fe P01) Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported by the manufacturer... |
|||
Tensile Strength, Yield | 280 - 350 MPa @Strain 0.200 % |
40600 - 50800 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 280YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Tensile Strength, Yield | >= 280 MPa | >= 40600 psi | |
SSAB Tunnplat Domex® 280XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Tensile Strength, Yield | >= 280 MPa | >= 40600 psi | |
SSAB Tunnplat Domex® 280YP Cold-forming Steel, HSLA Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®.. |
|||
Tensile Strength, Yield | 280 MPa | 40600 psi | 90º, RT, Dry; EN2561 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 280 MPa | 40600 psi | As Cast |
AFE Technologies Cronite 25Cr/12Ni No. HR7 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |
|||
Tensile Strength, Yield | >= 280 MPa | >= 40600 psi | |
AK Steel ASTM A 463 / SAE J1392 040 AHK, Grade 40 Aluminized Carbon Steel, Structural Steel (SS) Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 280 MPa | >= 40600 psi | |
AK Steel SAE J1392 040XLK or 040YLK, Grade 40 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 280 MPa | >= 40600 psi | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, HSLAS, FORMABLE 40K / SAE J1392 040 XLK or 040 YLK Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 280 MPa | >= 40600 psi | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 040XLK SAE Specified properties not covered by ASTMInformation provided by AK Steel |
|||
Tensile Strength, Yield | 280 - 340 MPa | 40600 - 49300 psi | |
ArcelorMittal Dual Phase 450 Very high strength steel, Cold Rolled Steel Available in the following: HCT500X (uncoated), HCT500X+ZE (electrogalvanized) and HCT500X+Z (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength and .. |
|||
Tensile Strength, Yield | 280 MPa @Strain 0.200 %, Temperature 538 °C |
40600 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Tensile Strength, Yield | 280 MPa @Strain 1.00 % |
40600 psi @Strain 1.00 % |
Typical after Solution Annealing |
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum.. |