Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 28.7 MPa | 4160 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® H5520 High Density Polyethylene ApplicationsALATHON H 5520 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include house.. |
|||
Tensile Strength, Yield | 28.7 MPa | 4160 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® M5040 High Density Polyethylene ApplicationsALATHON M 5040 is a copolymer with broad molecular weight distribution. This resin exhibits excellent color, low odor, and good processing stability. Typical applications for this res.. |
|||
Tensile Strength, Yield | 28.7 MPa | 4160 psi | ASTM D368 |
Reliance Industries PVAXX H60 The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie.. |