Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials F-244-S High Carbon Steel Powdered Metal Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-35All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials FCC-221-P Copper Steel Powdered Metal Applications:Medium strength mechanical componentsEquivalent MPIF Specification: FC-0205-35All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Pacific Sintered Materials FN-251-S Invar Powdered Metal Coefficient of thermal expansion equal to glass.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
PSM Industries Pacific Sintered Metals Copper Steel FC-221-P Powdered Metal Medium strength mechanical components Equivalent MPIF Specification: FC-0205-35Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Kinetics MIM F15 (Kovarâ„¢) Low CTE Alloy High nickel, high cobalt iron alloy. A traditional metal-to- glass sealing alloy that offers a low coefficient of thermal expansion (CTE) similar to glass. Provides the hermeticity required for firm.. |
|||
Tensile Strength, Yield | 276 - 379 MPa @Strain 0.200 % |
40000 - 55000 psi @Strain 0.200 % |
|
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 %, Temperature 538 °C |
40000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 276 - 483 MPa | 40000 - 70100 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Tensile Strength, Yield | 276 - 345 MPa @Strain 0.200 % |
40000 - 50000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Mueller Ecostream™ GreenDrop™ C27450 Lead Free Plumbing Brass As part of the Mueller Brass Company’s EcoStream™ family of alloys & products, GreenDrop™ C27450 Lead Free Brass is the ideal material solution for manufacturers required to comply wi.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | ASTM D638 |
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AEU PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include : Easy Molding, UV Stabilized. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East) LNP* VERTON* Is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
Heat Treated |
Universal Wire Works 410 Stainless Steel (AMS 5776) Filler Metal Universal 410 is a ferritic stainless steel alloy, primarily used as filler metal for gas metal arc and gas tungsten arc welding of steel of similar composition. Deposits are resistant to corrosion .. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | As Welded |
Universal Wire Works Inconel 92 (AMS 5675) Nickel Alloy Filler Metal Inconel Filler Metal 92 is a nickel base alloy designed especially for gas tungsten arc and gas metal arc welding of dissimilar combinations of high nickel alloys and austenitic and ferritic steels... |
|||
Tensile Strength, Yield | 276 - 359 MPa | 40000 - 52000 psi | |
Chicago Extruded Metals BioBrass® UNS C62400 Aluminum Bronze Finished product available as rod or forged.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | Premium Casting |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Carpenter Super Invar 32-5 Carpenter Super Invar 32-5, a magnetic, austenitic, solid solution alloy containing iron, nickel and cobalt, is designed to provide minimum thermal expansion at room temperatures. This alloy also e.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® 330 UNS N08330 Nickel Superalloy Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.Property values are for samples in the metallurgical condition: As rolled.Information provided by Allvac, An A.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® Grade 7 UNS R52400 Titanium Alloy Uses: Industrial components, CPI equipment, heat exchangers, pressure vessels, fittings, tubings.Property values are for samples in the metallurgical condition: 1300°F anneal.Information provided b.. |
|||
Tensile Strength, Yield | 276 MPa @Strain 0.200 % |
40000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 606 Nickel Superalloy Uses: Weld wire, woven wire mesh belts.Property values are for samples in the metallurgical condition: 2000°F anneal + water quench.Information provided by Allvac, An Allegheny Teledyne Company. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 0% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
Mueller Ecostream™ C36500 Uninhibited Leaded Muntz Metal As one of the lower lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36500 alloy provides a viable alternative to those manufacturers who are manufacturing produc.. |
|||
Tensile Strength, Yield | 276 MPa | 40000 psi | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-S Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-35Information Provided by Pacific Sintered Metals, a division.. |
|||
Tensile Strength, Yield | >= 276 MPa | >= 40000 psi | Minimum; longitudinal direction. (Transverse values generally lower). |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |
|||
Tensile Strength, Yield | >= 276 MPa | >= 40000 psi | Minimum |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |