Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.56 MPa | 3997 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Tensile Strength, Yield | 27.56 MPa | 3997 psi | |
C.O.I.M. PLAXTER® P 72 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
Tensile Strength, Yield | 27.56 MPa | 3997 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |