Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.3 MPa | 3960 psi | Formulation Example; Press Cure 7'/177ºC |
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot.. |
|||
Tensile Strength, Yield | 27.3 MPa | 3960 psi | Formulation Example; Press Cure 7'/177ºC |
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot.. |
|||
Tensile Strength, Yield | 27.3 MPa | 3960 psi | 65% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Toluene for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |