Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 255 MPa | 37000 psi | ASTM D638 |
PolyOne OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Strength, Yield | 255 - 300 MPa | 37000 - 43500 psi | With 0% cold work |
OMG Americas GlidCop® AL-15 Dispersion Strengthened Copper GlidCop® AL-15 is copper that is dispersion strengthened with 0.3 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o.. |
|||
Tensile Strength, Yield | 255 MPa @Strain 0.200 %, Temperature 649 °C |
37000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 255 - 352 MPa | 37000 - 51000 psi | 0.2% offset |
Eagle Brass 210 Gilding Metal, 1/2 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Yield | 255 MPa | 37000 psi | ASTM D638 |
Clariant Renol PPA1100G60 Polyphthalamide, 60% Glass Fiber Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 255 MPa @Strain 0.200 %, Temperature 204 °C |
37000 psi @Strain 0.200 %, Temperature 399 °F |
|
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Yield | >= 255 MPa | >= 37000 psi | |
AK Steel ZINCGRIP® 255, Grade 37 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 255 MPa @Strain 0.200 % |
37000 psi @Strain 0.200 % |
Typical; Annealed |
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600 Allegheny Ludlum is a nickel-chromium alloy designed for use from cryogenic to elevated temperatures in the range of 1093 degrees Celsius. AL 600 alloy is non-magnetic and readily weldable. The al.. |
|||
Tensile Strength, Yield | 255 MPa @Strain 0.200 %, Temperature 871 °C |
37000 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Tensile Strength, Yield | 255 MPa | 37000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PI-40CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |