Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Resirene Resirene® 2270 High Impact Polystyrene Features:Medium FlowGood GlossFDA Rating: 21 CFR 177.1640High ProductivityApplications:Extrusion/ ThermoformingInjectionDiskettesPen BarrelsInformation provided by US distributor Calsak Corporation... |
|||
Tensile Strength, Yield | 24.5 - 29.4 MPa | 3560 - 4270 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | ASTM D638 |
ExxonMobil HD 6761.17 Injection Molding Resin
(discontinued **) HD 6761 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a heavy-d.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
M. Holland Company CP710 Polypropylene Impact Copolymer AntistaticImpact copolymerGood flowGood impact resistanceNucleatedApplications: ClosuresHousehold goodsThin-walled parts |
|||
Tensile Strength, Yield | 24.5 MPa @Thickness 3.20 mm |
3560 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HI5204S PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 24.5 MPa @Thickness 3.20 mm |
3560 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HI5205R PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | |
Microcell Composite Company CELLIFF® 7000 Polymer Pellets CELLIFF® special high polymer materials are mixed for high degrees of hardness and tenacity. For producing stiff, light weight foaming boards which are tenacious and durable. The foam surface can.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® EPC40R Polypropylene impact copolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® SM340 Polypropylene impact copolymer Titanpro® SM340 is an intermediate impact material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adju.. |
|||
Tensile Strength, Yield | 24.5 MPa @Thickness 3.20 mm |
3560 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D1238 |
Iran Petrochemical (PCC) 7000F High Density Polyethylene 7000F is a high density polyethylene for enhanced ultra thin film.Information provided by Iran Petrochemical Commercial Co. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® FPC 20 PPC - 20% Calcium Carbonate Reinforced Polypropylene Copolymer 20% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® FPDZ-1000 - 25% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | ASTM D638M |
Total PSI 4440(AS) High Impact Polystyrene 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, .. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM Data |
Dow AIM® 4800 High Impact Styrenic Resin AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM Data |
Dow AIM® 4810 High Impact Styrenic Resin AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D-638 |
Bapolan® 6403 Polystyrene, Extrusion Grade Bapolan PS6403 is a high impact polystyrene resin designed for extrusion-thermoforming applications. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Applications: General purpose, housewar.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; Arlon SQA-TMS-008 |
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Arlon SQA-TMS-008 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Arlon SQA-TMS-008 |
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; Arlon SQA-TMS-008 |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; Arlon SQA-TMS-008 |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® FPDG-M FPDG M - 28% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CompoundApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP PP CO 220-23 Impact Polypropylene Copolymer PP CO 220-23 has easy mold flow and excellent dimensional stability. Applications include closures, housewares, and small appliance applications.Former A-Top Polymers product; part of Amco product l.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; ASTM E 831 |
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber.. |