Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 233 MPa @Strain 0.200 %, Temperature 204 °C |
33800 psi @Strain 0.200 %, Temperature 399 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Yield | 233 MPa | 33800 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10 LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |