Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 228 MPa | 33100 psi | ASTM D638 |
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Tensile Strength, Yield | 228 MPa @Strain 0.200 %, Temperature 316 °C |
33100 psi @Strain 0.200 %, Temperature 601 °F |
|
Haynes Hastelloy® G-30® alloy, plate and bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 CF30 30% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat.. |
|||
Tensile Strength, Yield | 228 - 241 MPa | 33000 - 35000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 X 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeighTPCI# 10065101Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6,6 GF50 HS L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF40 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedTPCI# 9627150Information provided by T.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® TPX-HTN-01040 A 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Tensile Strength, Yield | 228 MPa | 33100 psi | ISO 527 |
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 228 MPa @Strain 0.200 %, Temperature 316 °C |
33100 psi @Strain 0.200 %, Temperature 601 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 228 MPa @Strain 0.200 % |
33100 psi @Strain 0.200 % |
|
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Tensile Strength, Yield | 228 MPa @Strain 0.200 % |
33100 psi @Strain 0.200 % |
|
Carpenter Chrome Core® 8 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Tensile Strength, Yield | >= 228 MPa | >= 33100 psi | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Dent Resistant (DR 210) Compared to DS Type B, DR steels have higher initial YS which contributes to increased strength after forming.Information provided by AK Steel |
|||
Tensile Strength, Yield | 228 MPa @Strain 0.200 % |
33100 psi @Strain 0.200 % |
|
Carpenter Chrome Core® 8-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Tensile Strength, Yield | 228 MPa | 33100 psi | Offset not specified |
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Tensile Strength, Yield | 228 MPa | 33100 psi | |
AK Steel Aluminized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. DDS is made by adding aluminum to the molten steel and.. |
|||
Tensile Strength, Yield | >= 228 MPa | >= 33100 psi | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, AASHTO M218, CSP Information provided by AK Steel |
|||
Tensile Strength, Yield | 228 MPa @Strain 0.200 %, Temperature 538 °C |
33100 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Tensile Strength, Yield | 228 MPa @Strain 0.200 % |
33100 psi @Strain 0.200 % |
|
Carpenter Chrome Core® 12-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |