Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D638 |
S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant Application: A UL94 V-2, flame retardant polypropylene compound for injection molding applications, including cases for industrial power supply. Compound is designed with halogen-based flame retarda.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | at 100%; ASTM D412 |
5265 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D638 |
Resirene Resirene® 6220 High Impact Polystyrene Features:Low FlowEasy ProcessingGood GlossHigh ElongationFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Extrusion/ ThermoformingDisposablesGPPS/HIPS BlendsRefrigerator PartsInformation p.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® L43840U Rotational Molding LLDPE
(discontinued **) Butene CopolymerApplications: Toys and other non-tank rotational molding applications.Formolene L43840U is a Butene Copolymer of linear low density polyethylene for toys and other non-tank rotationa.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D638 |
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with DOP Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | Crosshead speed - 2" min; ASTM D638 |
LyondellBasell Alathon® M4661 High Density Polyethylene ApplicationsALATHON M 4661, formerly known as LYHD 060, exhibits excellent impact, warp and environmental stress crack resistance. Typical applications are closures, institutional seating and consum.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | Type I, 2 in/min; ASTM D638 |
M. Holland Company CP502 Polypropylene Copolymer Features: Copolymer, High Flow, High Impact ResistanceUses: Closures, Medical Applications, Thin-walled PartsProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM-D638 |
Ineos ABS Lustran® Guardian™ 732 ABS, Extrusion Grade Lustran® Guardian™ ABS 732 is an extrusion grade resin designed for use in thermoformed refrigerator and freezer liner applications. It is suitable for use with 245fa PU foams. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | 2 in/min.; ASTM D638 |
Ineos K44-15-122 HDPE K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D638 |
Ineos K44-15-123 HDPE Copolymer with Carbon Black Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D 638 |
LyondellBasell Pro-faxâ„¢ SG722 Polypropylene Copolymer Description: Pro-faxâ„¢ SG722 high flow, high impact polypropylene copolymer resin is designed for injection molding applications. This resin is available in pellet form. Pro-faxâ„¢ SG722 res.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-882 |
Saint-Gobain Norton® F710 Chemically Resistant Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: Chemical Resistant; Common in Electrical/ElectronicsInformation provided by Saint Gobain Performance Products. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Techmer ES HiFill® HIPS TM40 WT 40% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 40% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2"/min; ASTM D638 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 6613N Impact Copolymer Polypropylene Copolymer for Injection Molded Applications Requiring a Combination of High Toughness and Stiffness Formolene® 6613N is a copolymer of polypropylene designed and formulated for injection molding ap.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | aged 70 hours at 250ºF in ASTM Oil #901 |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
ExxonMobil HDPE BU46-060 High Density Polyethylene Resin Product Description: BU46-060 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ISO 527-2/1A/50 |
ExxonMobil HDPE HMA 016 High Density Polyethylene Resin Product Description: HMA 016 is a HDPE grade, characterized by fast cycling and good impact strength. It has high gloss and high dimensional stability.Availability: Africa & Middle East, Asia Pacifi.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 1901 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 4510 Flexible PVC Non-lead stabilized 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | Type I, 2 in/min; ASTM D638 |
M. Holland Company IS200 Polystyrene, High Impact
(discontinued **) Uses: Audio Tapes, Household Goods, ToysProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |