Polymer Property : Tensile Strength, Yield = 22.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.4 MPa
3250 psi
-20% change after 70 hours @ 100°C; ASTM D412
Precision Polymer Engineering Q75B Polyurethane Rubber
Sulphur cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG728, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist..
Tensile Strength, Yield 22.4 MPa
3250 psi
(2 in/min); ASTM D638
Phillips 66 COPYLENE® CM120LN Polypropylene Impact Copolymer
COPYLENE™ CM120LN is a high impact copolymer formulated with antistat and nucleated for demanding injection molding applications.Applications: Injection molding applications including crates, totes..
Tensile Strength, Yield 22.4 MPa
3250 psi
(2 in/min); ASTM D638
Phillips 66 COPYLENE® CM200LN Polypropylene Impact Copolymer
COPYLENE™ CM200LN has a superior balance of stiffness and impact strength. The high melt flow allows for quick filling of molds and the antistat and nucleation facilitates fast cycle times.Applicat..
Tensile Strength, Yield 22.4 MPa
3250 psi
ASTM D638
LyondellBasell Alathon® L5332CP High Density Polyethylene
ApplicationsALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resis..
Tensile Strength, Yield 22.4 MPa
3250 psi
ASTM D638
LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade
ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applic..
Tensile Strength, Yield 22.4 MPa
3250 psi
ASTM D638
Washington Penn Medium Impact Copolymer
Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array ..
Tensile Strength, Yield 22.4 MPa
3250 psi
at 100%; ASTM D412
Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane
Type: Estane® ALR CL650 is an aliphatic, polycaprolactone-based TPU with a Shore D Durometer of 65.Features: Contains a UV package that enhances outdoor weatherability. This high performance resin..
Tensile Strength, Yield 22.4 MPa
3250 psi
2.0 in/min; ASTM D638
ExxonMobil PP7855E1 Polypropylene Homopolymer
Product Description: A high crystallinity, medium impact strength copolymer resin with high melt flow rate and good processing attributes. It is designed for injection-molded automotive interior ap..
Tensile Strength, Yield 22.4 MPa
3250 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W1202 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne