Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.1 MPa | 3200 psi | at 100%; ASTM D412 |
1065D Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
M. Holland Company CP310 Polypropylene Impact Copolymer Impact CopolymerMedium flowHigh impact resistanceApplications: ClosuresInformation provided by M. Holland |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | Type I, 2 in/min; ASTM D638 |
M. Holland Company CP400 Polypropylene Copolymer Features: Medium Flow, High Impact ResistanceUses: Appliances, Business Equipment, Construction Applications, Tool/Tote Box, ToysProcessing Method: Injection MoldingInformation provided by M. Hollan.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | Type 1 Specimen, Rate: 2"/min; ASTM D638 |
Global GPP-2000 Polypropylene Impact Copolymer, Cold Temperature Impact Resistant, Nucleated Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 22.1 MPa @Temperature 23.0 °C |
3200 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos N07N-00 Polypropylene Impact Copolymer This is a medium melt flow rate, nucleated and antistatic impact copolymer polypropylene for injection molding applications that require a superior stiffness to impact balance.ApplicationsMaterials .. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | At 50 mm/min; ASTM D683 IV |
Borealis Borecene™ RM7403 Linear Polyethylene for Rotational Molding Borecene Compact RM7403 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2 in/min; ASTM D638 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2 in/min; ASTM D638 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2 in/min; ASTM D638 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
Total PSI 830 Polystyrene Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | |
Zylog Hipolyene® X2 DP 4 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 1-D Heavy Oil Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM Data |
Dow AIM® 4900 High Impact Styrenic Resin AIM® 4900 advanced styrenic resin for extrusion and thermoforming applications is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D-638 |
Axiall 8560 Moldings & Extrusions Flexible PVC A clear, semi-rigid extrusion or molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
Multibase Multi-Flam™ 0102 PP NH Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingCoextrusionExtrusionUses:TubingPipingFurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRDA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | at max load; ASTM D638 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2"/min; ASTM D638 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | Type I; ASTM D638 |
M. Holland Company IS325 Polystyrene, High Impact
(discontinued **) Features: Impact ModifiedUses: Construction Applications, Structural Foam, PackagingApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 22.1 MPa | 3200 psi | 2 in/min; ASTM D638 |
Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer PP CO 200 NB is cold temperature impact resistant, heat stabilized, and nucleated. Applications include toys and consumer products.Former A-Top Polymers product; part of Amco product line since 2013.. |