Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.5 MPa | 3120 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-0414 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-0616 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-061601 Description: Impact Modified PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 1402 TPO
(discontinued **) Description: SEQUEL® 1402 engineered polyolefin material is designed for large automotive exterior applications that require high melt flow, excellent paintability, and processability. Applications.. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 1493 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1493 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 5220 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 5220 engineered polyolefin is designed for large exterior applications that require superior painted gouge/scuff performance. This product also offers ductile impact propertie.. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | ASTM D638 |
Tipco Tipcolene® FPZ-CL - 10% Talc/Mineral Reinforced Polypropylene Copolymer Compound 10% Mineral Reinforced PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | ASTM D638 |
Tipco Tipcolene® ISRH 35 NF - 20% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow 20% Mineral Reinforced, PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP25-0616 Black Impact Modified Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | 50 mm/min |
Arkema Group Appryl® 3130 MU 7 Polypropylene - Polyethylene Copolymer PP/PE copolymer colored during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive industry. It .. |
|||
Tensile Strength, Yield | 21.5 MPa | 3120 psi | |
Radici Radilene® R 70 IE 5058 B High Density Polyethylene Shore hardness: 64 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a.. |