Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 20.2 MPa | 2930 psi | ASTM D412 |
Polymax® Maxelast® P3892 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 20.2 MPa | 2930 psi | ASTM D638 |
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b.. |
|||
Tensile Strength, Yield | 20.2 MPa | 2930 psi | Type IV specimen, 2" per minute test speed, 0.075" thickness compression molded samples; ASTM D 638 |
NOVA Chemicals Surpass® RMs341-U Octene sHDPE Rotational Molding Resin RMs341-U complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341-.. |
|||
Tensile Strength, Yield | 20.2 MPa | 2930 psi | Type IV specimen, 2" per minute test speed, 0.075" thickness compression molded samples; ASTM D 638 |
NOVA Chemicals Surpass® RMs341-UG Octene sHDPE Rotational Molding Resin RMs341-UG complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341.. |
|||
Tensile Strength, Yield | 20.2 MPa | 2930 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
LyondellBasell DEXFLEX® 940 TPO Description: DEXFLEX® 940 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior painted applications. Applications: Bumper fascias, claddings Information provided by .. |
|||
Tensile Strength, Yield | 20.2 MPa | 2930 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer Elastocon® SMR1600 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |