Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 20.0 MPa | >= 2900 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This m.. |
|||
Tensile Strength, Yield | >= 20.0 MPa | >= 2900 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + TLS Polyethylene Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | 50 mm/min; ISO/R 527 |
Okulen® 1000 PE-UHMW, Natural OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Petromont 7000 Medium Density Polyethylene Resin Petromont HDPE 7000 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is readily processed by blown sheet or flat die extrusi.. |
|||
Tensile Strength, Yield | 20.0 - 119 MPa @Temperature 100 - 175 °C |
2900 - 17300 psi @Temperature 212 - 347 °F |
Average value: 64.8 MPa Grade Count:8 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | 50 mm/min, 1/8" thick injection molded specimen; ISO 1183 |
Phillips Sumika Marlex® ABF-300 High Flow Thermoplastic Olefin
(discontinued **) Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Rotuba MS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 20.0 - 196 MPa | 2900 - 28400 psi | Average value: 131 MPa Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | |
LyondellBasell Lupolen® 3822 D GB 00350 MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638-02 |
Ipiranga Petrochem PCD 0810 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | |
Kuraray HYBRAR® HD1 Thermoplastic Rubber-HDPE Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Yield | 20.0 MPa @Temperature 23.0 °C |
2900 psi @Temperature 73.4 °F |
ISO 527-2/50 |
MBA Polymers HDPE 1107 E Post-consumer recycled fractional melt high density polyethylene Available in standard black.Information provided by MBA Polymers. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Kostat BK-STAT R048BK PS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ISO R527-1 |
LyondellBasell Hifaxâ„¢ CB228 Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good paintability, good processabilityApplications: aut.. |
|||
Tensile Strength, Yield | 20.0 - 35.0 MPa @Thickness 2.00 mm |
2900 - 5080 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | 50 mm/min; ASTM D638 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
UBE 7115U Nylon 6/12 Copolymer Description: UBESTA Nylon 12 CopolymerInformation provided by UBE. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM-D638 |
Polyram RamShine PV102 ABS, General Purpose General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | cond; ISO 527-1/-2 |
DSM Novamid® ST145 NAT PA6-I Impact Modified, Injection Molding |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | Molded property |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ISO R 527 |
Addiplast Addilene PMD 50215 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | |
BASF Procom® D 1146 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 20.0 MPa @Temperature 120 °C |
2900 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Tensile Strength, Yield | 20.0 MPa @Temperature 80.0 °C |
2900 psi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8253 PA6 (Conditioned) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Tensile Strength, Yield | 20.0 MPa @Temperature 80.0 °C |
2900 psi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Tensile Strength, Yield | 20.0 - 34.0 MPa | 2900 - 4930 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ISO 527 |
A.D. Compound Adene NCQAG Copolymer 40% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Tensile Strength, Yield | 20.0 - 79.3 MPa | 2900 - 11500 psi | Average value: 35.6 MPa Grade Count:21 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 20.0 - 30.0 MPa | 2900 - 4350 psi | Average value: 27.0 MPa Grade Count:7 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ISO 527 |
Unipetrol PE HD LITEN® ZB 20 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |