Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.62 MPa | 380 psi | at 200%, no post cure- press cured for 5 minutes; ASTM D412 |
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 2.62 MPa | 380 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-UR-110-W Polyurethane, Unspecified (PUR, Unspecified) Information provided by PolyOne |
|||
Tensile Strength, Yield | 2.62 MPa | 380 psi | ASTM D412 |
Polymax® Maxelast® P2750 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 2.62 MPa | 380 psi | @100% Elongation; ASTM D1414 |
Greene Tweed FLUORAZ® 784 Fluoroelastomer, FEPM Sanitary gaskets made from Fluoraz® 784 work well in Sip and CIP applications where a low durometer elastomer compound is needed. While EPDMs and FKMs can provide a seal for extended periods, ch.. |
|||
Tensile Strength, Yield | 2.62 MPa | 380 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5242 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | >= 2.62 MPa | >= 380 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7265D Fluorocarbon-Elastomer Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.62 MPa | 380 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7282 Neoprene / Chloroprene UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.62 MPa | 380 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7336 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.62 MPa @Strain 300 % |
380 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 36-021 NATURAL Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Specialty Thermoplastic ElastomerApplications: FDA (Food Contact)Processing Method: Injection MoldingInformation provided by PolyOne Corporation |