Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.52 MPa @Strain 300 % |
365 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3945 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |