Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G92A Perfluoroelastomer An electrically conductive black perfluoroelastomer with excellent chemical and steam resistance.Applications: Specially formulated for applications requiring special electrical properties. Origina.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D412 |
Precision Polymer Engineering R70Z Natural Rubber Natural Rubber, 65-75 °IRHD. Formulated to meet BS1154 Grade Z70. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Tensile Strength, Yield | 19.0 - 28.0 MPa | 2760 - 4060 psi | |
Reliance Industries Polypropylene Impact Copolymer Typical properties of Reliance - Repol Polypropylene grades. Properties depend on rubber content, presence of nucleating agent, MFIInformation provided by Reliance Industries |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 19.0 MPa @Temperature 23.0 °C |
2760 psi @Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Tensile Strength, Yield | 19.0 - 63.0 MPa @Temperature -40.0 - 80.0 °C |
2760 - 9140 psi @Temperature -40.0 - 176 °F |
Average value: 41.0 MPa Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
Chevron Phillips HiD® 9301 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234360A; ASTM D 4976 Classification: PE 225, A 56607Applications:Base Resin for use in Gas, Oil Patch and Industrial Pipe.. |
|||
Tensile Strength, Yield | 19.0 - 82.7 MPa | 2760 - 12000 psi | Average value: 46.0 MPa Grade Count:35 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer INNOPOL® CS 2-3302 TO BU is an elastomer modified, UV-stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3302 TO BU is developed for producing injection molded automotive.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
LyondellBasell Astryn BB725GC Polypropylene Copolymer, Mineral Filled Key Features: medium melt flow, medium high modulus, UV-stabilized, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good processability, good weatherability,Applicati.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527-1, -2 |
LyondellBasell Hostacomâ„¢ BG749GC/1 Polypropylene Copolymer Description: Hostacomâ„¢ BG749GC/1 medium melt flow, 1,100 MPa flexural modulus, UV-stabilized, precolored, 20% calcium carbonate-filled polypropylene copolymer resin has an excellent combination.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AFB42 ABS LNP* THERMOCOMP* AFB42 is a compound based on ABS containing 10% Glass Fiber, 20% Glass Bead. |
|||
Tensile Strength, Yield | 19.0 MPa | 2750 psi | ASTM D412 |
Teknor Apex APEX® 3302-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 19.0 MPa @Temperature 80.0 °C |
2760 psi @Temperature 176 °F |
ISO Data |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Tensile Strength, Yield | 19.0 MPa @Temperature 80.0 °C |
2760 psi @Temperature 176 °F |
ISO Data |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength, Yield | 19.0 MPa | 2750 psi | ASTM D638 |
Washington Penn Medium Impact Copolymer 20% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 2.0 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EB6400 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 Type IV |
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: geomembrane, gas and chemical containment liners, landfill linersInfor.. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 50.0 % |
2760 psi @Strain 50.0 % |
|
Covestro Texin® 260 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | |
Dow DOWLEX™ IP-42 High Density Polyethylene DOWLEX® IP-42 resin is an improved processing high density polyethylene resin designed for excellent flow and high impact. DOWLEX IP-42 resin is designed by optimizing the breadth and shape of the .. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
Dow DS6D82 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D82 Polypropylene Resin is intended for use as a heat seal coati.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
Braskem CP 195 Injection Molding Polypropylene Description: CP 195 is a very high melt flow rate heterophasic copolymer developed for high speed injection moulding machines and high productivity thin-walled injection moulded parts. The product f.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM-D638 |
Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer IN34 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibil.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 2 in/min, specimen injection molded by ASTM method D1897; ASTM D638 |
Chevron Phillips K-Resin® BK18 Styrene-Butadiene Copolymer
(discontinued **) Characteristics: Good flexibilityGood impact resistanceGood clarityGood mold releaseApplications: ToysOvercapsConsumer productsInformation provided by Chevron Phillips. |
|||
Tensile Strength, Yield | 19.0 MPa | 2750 psi | ASTM D-638 |
Axiall 390 Coax & Telecom Flexible PVC Buried service telecom jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 2.0 in/min; ASTM D638 |
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2750 psi | ASTM D-638 |
Axiall 15900 Wire & Cable Flexible PVC Non-lead stabilized insulation compound recommended for TW and 80C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |