Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.5 MPa | 2690 psi | ASTM D412 |
Polymax® Maxelast® P3991 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 18.5 MPa | 2680 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G81T Perfluoroelastomer A special black perfluoroelastomer compound with PTFE blended for improved mechanical performance. Excellent steam resistance and mechanical properties. Extremely low outgassing properties. Applica.. |
|||
Tensile Strength, Yield | 18.5 MPa | 2680 psi | ASTM D638 |
Reliance Industries Relene W43006 Polyethylene Relene W43006 is a polyethylene grade recommended for insulation in jelly filled telecommunication cables. This grade contains a special stabilization system for improved thermal resistance. It is.. |
|||
Tensile Strength, Yield | 18.5 MPa | 2690 psi | ASTM D412 |
Teknor Apex APEX® 90-A41R-80-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 18.5 MPa | 2680 psi | ASTM D412 |
Teknor Apex APEX® 90-A472R-85-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Tensile Strength, Yield | 18.5 MPa | 2680 psi | ASTM D412 |
Teknor Apex ELEXAR® EL 8623 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 18.5 MPa | 2680 psi | ASTM D412 |
Teknor Apex Flexalloy® 9300-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Tensile Strength, Yield | 18.5 MPa | 2680 psi | ASTM D638 |
Tipco Tipcolene® HR 8234 - 10% Talc/Mineral Reinforced Polypropylene Copolymer, Very High Impact Strength & Flow 10% Mineral Reinforced, Very High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 18.5 MPa | 2680 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea.. |
|||
Tensile Strength, Yield | 18.5 MPa | 2680 psi | ASTM D-638 |
Axiall 17870 Wire & Cable Flexible PVC TW, THW insulation compound. Oil II rated. 720 hour sunlight resistant in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |