Polymer Property : Tensile Strength, Yield = 171 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 171 MPa
24800 psi
ASTM D638
Omni Plastics OmniLon™ 6 PA6 GR33 NA Glass Reinforced Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Tensile Strength, Yield 171 MPa
24800 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXS PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFL36SXS is a compound based on PA 66 resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.
Tensile Strength, Yield 171 MPa
24800 psi
ISO 527
Eurostar Star L PA66 30V D51 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D51 is a PTFE lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.