Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.93 MPa | 2601 psi | 10% change after 70 hours @ 150°C; ASTM D412 |
Precision Polymer Engineering Z70B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Butadiene Rubber (HNBR), 65-75 °IRHD. Medium acrylonitrile content (ACN = 34%). To meet ASTM D2000/SAE J200 line call-out M4DH716, A26, B36, EO16, EO36, F17.A.. |
|||
Tensile Strength, Yield | 17.93 MPa | 2600 psi | 2.0 in/min; ASTM D638 |
ExxonMobil LL 8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Tensile Strength, Yield | 17.93 MPa | 2600 psi | 2.0 in/min; ASTM D638 |
ExxonMobil LLP8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |