Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 0850-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JD455CJ Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WJAF111L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 1490 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1490 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D638 |
M. Holland Company LL800 LLDPE
(discontinued **) Features: Fast Production Cycle, High Gloss, Low Temp. Impact Resistance, Low to No Odor, Low WarpageUses: Containers, Household Goods, Lids, Thin-walled PartsApprovals: FDA 21 CFR 177.1520(c) 3.2a .. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R3790B Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D638 |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 16.5 MPa @Temperature 23.0 °C |
2390 psi @Temperature 73.4 °F |
ISO 527-2/50 |
MBA Polymers PP 2182 Post-consumer recycled polypropylene copolymer Very high melt flow rate for injection molding application. Available in standard black.Information provided by MBA Polymers. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D638 |
Multibase Multi-Flamâ„¢ 2903 LDPE Polyethylene Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D638 |
Techmer ES HiFill® PP GB60 60% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex APEX® 3302-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | Longitudinal |
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.008" thick) Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Chevron Phillips Marlex® 5104 LDPE Blow Molding Resin Resin Type: HomopolymerCharacteristics: High Melt Strength, Good Parison Control, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on Gloss, Long Standing .. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMU130P Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ISO 527-1/-2 |
DSM Arnitel® UM551-V Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | >= 16.5 MPa | >= 2400 psi | ASTM D638 |
Buckeye Polymers BP FLEX D5718 TU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 01560 Plenum Flexible PVC CAT 5 rated plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 113B-FR Moldings & Extrusions Flexible PVC Non-lead stabilized, 105°C rated injection molding compound. Rated 94 V-0 at 1.5 mm and 94 V-1 at 0.58 mm for all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 8830 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, shapes, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 8870 Moldings & Extrusions Flexible PVC Economical general purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 19853 Wire & Cable Flexible PVC Non-lead stabilized insulation compound recommended for 105°C applications 1/32 wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.5 - 31.0 MPa | 2390 - 4500 psi | Average value: 23.3 MPa Grade Count:116 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledUV StabilizedApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First Choic.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 18840 Wire & Cable Flexible PVC Non-lead stabilized 105C jacket compound for use in SPTO, SJTO and SVTO applications. Best suited for 30 mil walls and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |