Polymer Property : Tensile Strength, Yield = 150.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 150.00 MPa
21755 psi
ASTM D638
Fiberfil® FPI-33 BK Nylon 6, 33% Glass Reinforced, post industrial
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 150.00 MPa
21755 psi
ASTM D638
Fiberfil® FV-30 Nylon 6, 30% Glass Reinforced, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 150.00 MPa
21755 psi
ASTM D638
Fiberfil® FV-31 Nylon 6, 31% Glass Reinforced, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics