Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 147 MPa | 21300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin Extem XH2315 Resin |
|||
Tensile Strength, Yield | 147 MPa | 21300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific) Extem XH2315 Resin |
|||
Tensile Strength, Yield | 147 MPa | 21300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East) Extem XH2315 Resin |
|||
Tensile Strength, Yield | 147 MPa @Thickness 3.20 mm |
21300 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 147 MPa @Thickness 3.20 mm |
21300 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 147 MPa @Thickness 3.20 mm |
21300 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Tensile Strength, Yield | 147 MPa | 21300 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 GF33 TS15 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Tensile Strength, Yield | 147 MPa | 21300 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2165MC PPS Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 147 MPa | 21300 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2165MC PPS Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 147 MPa | 21300 psi | ASTM D638 |
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |