Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.46 MPa | 2097 psi | ASTM D638 |
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |