Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1380 MPa | 200000 psi | 50% Cold Rolled |
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
Tensile Strength, Yield | 1380 MPa @Strain 0.200 % |
200000 psi @Strain 0.200 % |
Aged to ~ 46 HRC |
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli.. |
|||
Tensile Strength, Yield | 1380 MPa | 200000 psi | R<sub>p</sub>02. short transverse direction. 48 HRC. |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |