Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527, ASTM D638 |
Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527-1/2 |
Radici Radilon® SERV3808 K (dry) Nylon 6 Heat stabilized glass-fiber reinforced with high impact strengthInformation provided by Radici group. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, at 50% RH
&n AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
PTS Trimid® N6-TG30L-BK 30% Glass Fiber, High Impact Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 130 - 280 MPa | 18900 - 40600 psi | |
Materion Beryllium Copper Alloy 25 Forgings & Extrusions; A (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 - 250 MPa | 18900 - 36300 psi | |
Materion Beryllium Copper Alloy 25 Tube; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Tensile Strength, Yield | 130 MPa @Temperature 550 °C |
18900 psi @Temperature 1020 °F |
Annealed prior to test |
Special Metals INCOLOY® Alloy 800HT™ A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527 |
Polyram PlusTek PD305G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced Nylon 12 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | >= 130 MPa | >= 18900 psi | ASTM-D638 |
Polyram PlusTek RB300G6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM-D638 |
Polyram PlusTek RD302G6 Nylon 12, 30% Glass Fiber 30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM-D638 |
Polyram RamSter PF300G6 PBT, 30% Glass Fiber 30% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527 |
Polyram RamSter PF305G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM-D638 |
Polyram RamTough PZ300G6 Polycarbonate, 30% Glass Fiber 30% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM-D638 |
Polyram PlusTek RA307G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | D638 |
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECA.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
E-Polymers TEKAMID® TA210SG30 Impact Modified, 30% Glass Fiber Reinforced PA66, DAM 30% Glass Fiber reinforced, Impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
E-Polymers TEKANATE™ G715FR , Flame Retardant, 15% Glass Fiber Reinforced Poly Carbonate 15% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
E-Polymers Tekaloy® T80GFR , Flame Retardant, 30% Glass Fiber Reinforced PBT/ABS Alloy 30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 50 mm/min; ISO 527-2 |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT Description: Is a PBT, injection-molding grade with 30% glass fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance, e.g. automotive connect.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® A3X4G7 BK 23079 35% Glass Filled PA66 FR (Dry) Description: 35% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stiffness and stre.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Tensile Strength, Yield | 130 MPa @Strain 0.200 % |
18900 psi @Strain 0.200 % |
|
ALIMEX ACP 5080R Aluminum Cast Material Sizes range availability along with good mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.Information .. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, Conditioned Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527 |
Polyram PlusTek RA320G5 Nylon 66 for Injection Molding, 25% Glass-Fiber Reinforced, Flame Retardant and High Stiffness 25% Glass-fiber reinforced, flame retardant and high stiffness Nylon 66 for injection molding applications.Information provided by Polyram. |