Polymer Property : Tensile Strength, Yield = 1207 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1207 MPa
175100 psi
Latrobe Lescalloy® HY-180 VIM-VAR ; 2.01 - 4.00 thickness High Strength Alloy Steel
LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superi..
Tensile Strength, Yield 1207 MPa

@Strain 0.200 %
175100 psi

@Strain 0.200 %
Carpenter Custom 450® Stainless Steel, 25 mm Bar, Condition H1050 (Age Hardened 566°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Yield 1207 MPa

@Strain 0.200 %
175100 psi

@Strain 0.200 %
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction + Aged 538°C (1000°F)/4hr/AC
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..
Tensile Strength, Yield 1207 MPa

@Strain 0.200 %
175100 psi

@Strain 0.200 %
ATI Allegheny Ludlum AL 13-8™ H 1025 Precipitation Hardening Alloy
Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t..