Tensile Strength, Yield 1190 MPa

@Strain 0.200 %
173000 psi

@Strain 0.200 %
Haynes 230® alloy, 40% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..