Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1160 - 1270 MPa | 169000 - 184000 psi | 3/4"x 0.030" Fiberglass Reinforced |
Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements GoldMemberâ„¢ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and.. |
|||
Tensile Strength, Yield | 1160 MPa @Strain 0.200 % |
168000 psi @Strain 0.200 % |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 35% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |