Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1103 MPa | >= 160000 psi | 0.2% proof |
Kobe Steel KS15-5-3 Beta Titanium Alloy, AMS 4914, Solution treated and aged, Forgings Nominal Composition: Ti-15 Mo-5 Zr-3 AlApplications: Implant materials for orthopedics, erosion shields, gold club heads. Features:Super high strength.Information provided by Kobe Steel |
|||
Tensile Strength, Yield | >= 1103 MPa | >= 160000 psi | 0.2% proof |
Kobe Steel KS-6-2-4-6 Alpha-Beta Titanium Alloy, AMS 4981, Solution treated and aged. Thickness ≤ 3 in. Nominal Composition: Ti-6 Al-2 Sn-4 Zr-6 Mo Applications: Jet engine parts. Features:High strength, excellent balance between strength and toughness.Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 1103 MPa | 160000 psi | 177°C Temper Temperature |
Latrobe Lescalloy® 16NCD13 VAC-ARC High Strength Alloy Steel 16NCD13 VAC-ARC is a premium quality low alloy, carburizing casehardenable vacuum arc remelted steel which takes its name from the French industry designation. In the carburized condition, its high .. |
|||
Tensile Strength, Yield | 1103 MPa @Strain 0.200 %, Temperature -18.0 °C |
160000 psi @Strain 0.200 %, Temperature -0.400 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 1103 MPa @Temperature -54.0 °C |
160000 psi @Temperature -65.2 °F |
Offset not given |
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |