Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 110.3 MPa | 16000 psi | ASTM D638 |
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 110.3 MPa @Thickness 3.17 mm |
16000 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |