Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1069 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age Data provided by Allvac.Applications: Compressor discs, heavy section forgings for gas turbine engine components. High tensile strength and good fracture toughness. |
|||
Tensile Strength, Yield | 1069 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 15-5 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age Data provided by Allvac.Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts. |
|||
Tensile Strength, Yield | 1069 MPa @Strain 0.200 % |
155000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 17-4 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age Data provided by Allvac.Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts. |
|||
Tensile Strength, Yield | 1069 MPa | 155000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 60% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 1069 MPa | 155000 psi | |
HP Alloys Alloy 718, 25% Cold Worked 25% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |