Polymer Property : Tensile Strength, Yield = 1068 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 1068 MPa

@Strain 0.200 %
>= 154900 psi

@Strain 0.200 %
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5),
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to
Tensile Strength, Yield 1068 MPa
154900 psi
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STOA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STOA (885°C/1hr/AC + 705°C/1hr/AC) condition. Other data below are typical of TIMETAL..