Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1060 - 1170 MPa | 154000 - 170000 psi | Solution Annealed & Aged |
Materion Beryllium Copper Alloy 245C Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Tensile Strength, Yield | 1060 - 1380 MPa | 154000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 1060 - 1350 MPa | 154000 - 196000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 1060 - 1350 MPa | 154000 - 196000 psi | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 1060 - 1350 MPa | 154000 - 196000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 1060 - 1210 MPa | 154000 - 175000 psi | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM08 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 1060 - 1170 MPa | 154000 - 170000 psi | Solution Annealed & Aged |
Materion Beryllium Copper Alloy 245CT Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Tensile Strength, Yield | 1060 MPa @Strain 0.200 % |
154000 psi @Strain 0.200 % |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |